• XH-31A (low temperature resistance, low temperature brittleness up to -40 ℃)
XH-31A (low temperature resistance, low temperature brittleness up to -40 ℃)
+

XH-31A (low temperature resistance, low temperature brittleness up to -40 ℃)

This material is based on chlorinated polyethylene

Still deciding? Get the samples first,Contact us!

XH-31A (low temperature resistance, low temperature brittleness up to -40 ℃)

This material is based on chlorinated polyethylene

Still deciding? Get the samples first,Contact us!

  • Description
  • Product Description 
    This material is based on chlorinated polyethylene and mixed with other additives. It has excellent flame retardancy, low temperature resistance, low smoke, earthquake resistance, radiation resistance, and outstanding mechanical properties. It is an ideal substitute for rubber sheaths based on chloroprene rubber and chlorosulfonated polyethylene rubber. This product fully meets the technical requirements of GB/T29631-2013 standard and can also adapt to the special working environment of wind power plants. 
    Product Usage 
    Suitable for single core wind energy flexible cables with ethylene propylene insulation and chlorinated polyethylene sheath for AC rated voltage of 1.8/3kv and below. 
    Overall performance indicators

    Performance index

    Company

    Typical values

    Mechanical properties before aging

     

     

    Tensile strength

    MPa

    13.5

    Elongation at break

    %

    360

    SHORE hardness

    A

    74

    Tear resistance performance

    N/mm

    9.0

    70 ℃, 240h thermal aging

     

     

    Change rate of tensile strength

    %

    8

    Change rate of elongation at break

    %

    -9

    Hardness change rate

    %

    16

    Mineral oil immersion at 100 ℃ for 24 hours

     

     

    Change rate of tensile strength

    %

    -5

    Change rate of elongation at break

    %

    -10

    Hardness change rate

    %

    -31

    Thermal extension test

     

     

    Test temperature

    200

    Test time

    min

    15

    Load

    MPa

    0.2

    Elongation under load

    %

    35

    Permanent deformation after cooling

    %

    6

    Low temperature bending

     

     

    Test temperature

    -35

    Test time

    h

    16

     

     

    No cracks

    Low temperature brittleness

    -40

    Bending experiment

    300000 times

    No cracks

    Processing process parameters 
    It is recommended to use CV (continuous vulcanization) production line for extrusion production. 
    Extruder compression ratio: 1.1:1 to 1.5:1;   
    Length to diameter ratio: 6:1 to 16:1 or higher (hot feeding is recommended for ratios below 10:1); 
    Extruder temperature: 65-85 ℃;   
    Sulfurization tube temperature: 165-185 ℃.  
    Packaging and Storage 
    The material has a rectangular film shape (which can also be packaged and changed according to user requirements), and should be stored in a clean, dry, and ventilated warehouse.

Query now

Note: Please leave your email address and our professionals will contact you as soon as possible!