This material is based on chlorinated polyethylene

Still deciding? Get the samples first,Contact us!

XH-00A (65 ° C general rubber sheath)

This material is based on chlorinated polyethylene

Still deciding? Get the samples first,Contact us!

  • Description
  • Product Description
    This material is based on chlorinated polyethylene and mixed with other additives. It has flame retardancy, oil resistance, wear resistance, tear resistance, cold resistance, weather resistance, and good mechanical properties. Equivalent to the XH-00A type sheath in GB7594-87 standard and the SE3 type sheath rubber in GB5013.1-2008, which is a general rubber sheath at 65 ° C. Due to its excellent performance, good extrusion appearance, and low cost, it has become an ideal substitute for rubber sheaths based on chloroprene rubber and chlorosulfonated polyethylene rubber.
    Product Usage
    Used for the outer sheath of YZ, YC, RQ cables in general rubber sheathed cable products.
    Comparison of material properties and standard requirements

    Experimental project

    Unit

    GB7594-87 XH-00A

    GB5013.1-2008 SE3

    Typical values

    Mechanical properties before aging

     

     

     

     

    Tensile strength

    MPa

    ≥7.0

    ≥7.0

    8.5

    Elongation at break

    %

    ≥300

    ≥300

    420

    75 ° C, mechanical properties after 10 days of aging

     

     

     

     

    Change rate of tensile strength

    %

    -20 ~ +20

    -20 ~ +20

    2.5

    Change rate of elongation at break

    %

    -20 ~ +20

    -20 ~ +20

    -7.8

    Thermal extension test

     

     

     

     

    Experimental conditions

    Test temperature

    °C

    200

    200

     

    Load time

    min

    15

    15

     

    Mechanical stress

    MPa

    0.2

    0.2

     

    Elongation under load

    %

    ≤175

    ≤175

    13

    Permanent deformation after cooling

    %

    ≤25

    ≤25

    8.6

    Processing process parameters
    It is recommended to use CV (continuous vulcanization) production line for extrusion production.
    Extruder compression ratio: 1.1:1 to 1.5:1;
    Extruder length to diameter ratio: 6:1 to 16:1 (if it is less than 10:1, it is recommended to use hot feed);
    Extruder temperature: 65-85 ℃;
    Sulfurization temperature: 165-185 ℃.
    Packaging and Storage
    The material has a rectangular film shape (which can also be packaged and changed according to customer requirements), and should be stored in a clean, dry, and ventilated warehouse.