• XJ-30A (125 ℃ medium voltage ethylene propylene rubber insulation material)
XJ-30A (125 ℃ medium voltage ethylene propylene rubber insulation material)
+

XJ-30A (125 ℃ medium voltage ethylene propylene rubber insulation material)

This material is based on EPDM rubber.

Still deciding? Get the samples first,Contact us!

XJ-30A (125 ℃ medium voltage ethylene propylene rubber insulation material)

This material is based on EPDM rubber.

Still deciding? Get the samples first,Contact us!

  • Description
  • Product Description 
    The XJ-30A type 125 ℃ medium voltage ethylene propylene rubber insulation material produced by our company is based on ternary ethylene propylene rubber as the basic material, supplemented with reinforcing agents, softeners, fillers, anti-aging agents, vulcanizing agents, etc., fully mixed by an internal mixer. The insulation layer of medium voltage cables used in mining, marine and other industries meets the requirements of the XJ-30A type product in GB7594-87 standard, and has excellent process performance. 
    Product Usage 
    This product can be used as insulation material for marine cables and mining cables with a voltage of 6 kV and below, and can be used for a long time at temperatures ranging from -40 to 90 ℃. This material has high flexibility, is easier to bend and move, and is convenient for cable installation and laying. The color is originally white, but other color products can also be provided according to user requirements. 
    Overall performance indicators

    Test project

    Company

    Typical values

    Mechanical properties before aging 
    Tensile strength 
    Elongation at break

    MPa 
    %

    8.9 
    364

    Mechanical properties of air box after aging at 158 ℃ for 168 hours 
    Retention rate of tensile strength 
    Retention rate of elongation at break

    % 
    %

    109 
    83

    Electrical performance

     

     

    Volume resistivity at room temperature

    Ω·cm

    2.8×1015

    Breakdown strength

    kv/mm

    25.5

    Mooney viscosity ML (1+4), 100 ℃

     

    53

    Burning time (T5120 ℃)

    min

    >20

    Processing process parameters
    It can be extruded and produced on a regular rubber extruder, and it is recommended to use a CV (continuous vulcanization) production line.
    Extruder compression ratio: 1.1:1 to 1.5:1;
    Extruder length to diameter ratio: 6:1 to 16:1;
    Temperature setting: 70-90 ℃
    Sulfurization temperature: It is recommended to maintain a temperature of 180-200 ℃ inside the vulcanization tube
    Packaging and Storage
    The product is packaged in cardboard boxes and lined with polyethylene bags. The film shape is continuous film or provided according to user requirements, with a net weight of 25Kg per box and 20 bags as one supply unit. The safe use period at room temperature is one year. The product should be stored in a clean, dry, cool, and ventilated warehouse.

Query now

Note: Please leave your email address and our professionals will contact you as soon as possible!